CLIN 0001: Apply Chromium Nitride Coating Spindles
FFP
Apply Chromium Nitride Coating to outside of Spindles per Drawing 11583062
and Statement of Work.
Apply Chromium Nitride Coating at process temperature 975°F
A: Surface prep: Prior to and post Chromium Nitride application critical surfaces to
meet surface finish Ra<16 Non-Critical surfaces to meet surface finish Ra<63.
B: Surface Thickness .0002-.0005
C: Hardness HV>2000
D: Adhesion Per ASTM B571 Method 13.1
E: CORROSION, ISO 4628-1 RATING = 5 FOLLOWING 250 HOURS
CYCLICAL CORROSION TESTING PER GMWI 4872.
Pricing Based on Estimated Quantity of 100 Pieces shipped at estimated quantity
of 10 per month.
Please provide pricing as follows:
Price per Piece; $_______
Price per lot of 10: $_______
All return shipping, packing and handling charges to be included in above pricing.
*Any unused funds will be deobligated prior to contract closeout*
Service Contract Labor Standards 15-4143 Latest Revision applies and is
incorporated.
Certificate of Conformance is required with every return shipment per COC CN5.
Contracting Officer's Representative: Julie Cannon
Amendment 0001 issued to add CLINs 0002 and 0003 for an additional 8 Spindles each. See attachment.
All interested offerors must sign the amendment document and return to the POC listed.