1 LOT - Apply Chromium Nitride Coating Spindles
FFP
Apply Chromium Nitride Coating to outside of Spindles per Drawing 11583062 per Statement of Work
Apply Chromium Nitride Coating at process temperature 975°F
A: Surface prep: Prior to and post Chromium Nitride application critical surfaces to meet surface finish Ra<16 Non-Critical surfaces to meet surface finish Ra<63.
B: Surface Thickness .0002-.0005
C: Hardness HV>2000
D: Adhesion Per ASTM B571 Method 13.1
E: CORROSION, ISO 4628-1 RATING = 5 FOLLOWING 250 HOURS CYCLICAL CORROSION TESTING PER GMWI 4872.